Statistical analysis of yield strength spectrum from nanoindentation for identification of constituent phases in steel

Author(s):

Medium: journal article
Language(s): English
Published in: IOP Conference Series: Materials Science and Engineering, , v. 869
Conference: XXIII International Scientific Conference on Advance in Civil Engineering: "CONSTRUCTION - THE FORMATION OF LIVING ENVIRONMENT" (FORM-2020) 23-26 September 2020, Hanoi, Vietnam
Page(s): 052038
DOI: 10.1088/1757-899X/869/5/052038
Structurae cannot make the full text of this publication available at this time. The full text can be accessed through the publisher via the DOI: 10.1088/1757-899X/869/5/052038.
  • About this
    data sheet
  • Reference-ID
    10432015
  • Published on:
    25/08/2020
  • Last updated on:
    25/08/2020
 
Structurae cooperates with
International Association for Bridge and Structural Engineering (IABSE)
e-mosty Magazine
e-BrIM Magazine