Role of crack-tip residual stresses in stress corrosion behaviour of prestressing steel

Author(s):
Medium: journal article
Language(s): English
Published in: Construction and Building Materials, , n. 5, v. 12
Page(s): 283-287
DOI: 10.1016/s0950-0618(98)00010-5
Structurae cannot make the full text of this publication available at this time. The full text can be accessed through the publisher via the DOI: 10.1016/s0950-0618(98)00010-5.