A review on the mechanical properties of cement-based materials measured by nanoindentation

Author(s):

Medium: journal article
Language(s): English
Published in: Construction and Building Materials, , v. 90
Page(s): 80-90
DOI: 10.1016/j.conbuildmat.2015.05.008
Structurae cannot make the full text of this publication available at this time. The full text can be accessed through the publisher via the DOI: 10.1016/j.conbuildmat.2015.05.008.