Performance and strength calculation of CFST columns with localized pitting corrosion damage

Author(s):



Medium: journal article
Language(s): English
Published in: Journal of Constructional Steel Research, , v. 188
Page(s): 107011
DOI: 10.1016/j.jcsr.2021.107011
Structurae cannot make the full text of this publication available at this time. The full text can be accessed through the publisher via the DOI: 10.1016/j.jcsr.2021.107011.