Effect of dry/wet ratio and pH on the stress corrosion cracking behavior of rusted X100 steel in an alternating dry/wet environment

Structurae cannot make the full text of this publication available at this time. The full text can be accessed through the publisher via the DOI: 10.1016/j.conbuildmat.2020.120478.