Comparison of Unconfined‐ and Confined‐Creep Tests for Hot Mix Asphalt

Author(s):

Medium: journal article
Language(s): English
Published in: Journal of Materials in Civil Engineering (ASCE), , n. 2, v. 6
Page(s): 307-326
DOI: 10.1061/(asce)0899-1561(1994)6:2(307)
Structurae cannot make the full text of this publication available at this time. The full text can be accessed through the publisher via the DOI: 10.1061/(asce)0899-1561(1994)6:2(307).